Jump to content

Specific Process Knowledge/Etch: Difference between revisions

From LabAdviser
Khr (talk | contribs)
Khr (talk | contribs)
Line 23: Line 23:
*[[/Etching of Silicon Oxide|Silicon Oxide]]
*[[/Etching of Silicon Oxide|Silicon Oxide]]
*[[/Etching of Bulk Glass|Bulk Glass]] - ''Borofloat (pyrex) and fused silica (quartz)''
*[[/Etching of Bulk Glass|Bulk Glass]] - ''Borofloat (pyrex) and fused silica (quartz)''
*[[/IBE magnetic stack etch|Magnetic stack containing Ta/MnIr/NiFe etch]]
*[[Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300/IBE magnetic stack etch|Magnetic stack containing Ta/MnIr/NiFe etch]]


== Choose a dry etch equipment ==
== Choose a dry etch equipment ==

Revision as of 10:04, 10 December 2012

Wet etch or dry etch

Etching at Danchip can be done either with wet chemistry or in dry etch equipment. In general wet chemistry etches isotropically in most materials were as dry etch techniques can be optimized to transfer a given mask pattern with vertical sidewalls (anisotropically) to a given substrate.

Advantages of wet chemistry over dry etch techniques are:

  • An often high etch rate difference of different materials giving raise to a high selectivity of the material to be etched compared to underlaying layers or mask materials.
  • Time saving: You can often etch 25 wafers at a time in wet chemistry where as dry etch equipment can only handle one wafer at a time.
  • Easy to start op new etch solutions.

Advantages of dry etch over wet chemistry:

  • Anisotropic etch can be done.
  • The etch do not attach the backside of the sample.

Choose material to be etched

Choose a dry etch equipment

Choose a wet etch