For 5" masks:


Lyngby 12.07.19
All Layers:
	5" chromium mask
	fracture limits ((-50000, -50000),(50000, 50000))
	Dark periphery
	Chromium down

GDS-file: GLO006_v7.gds
Top cell: wafer

Layer (GDS number): 01 
Mask Type: Digitised data= Dark, right reading
Text(max 30 characters): init-2019-Nitride-etch

Layer (GDS number): 02
Mask Type: Digitised data= Clear, Wrong reading
Text(max 30 characters): init-2019-KOH-backside


Yours sincerely 
Nancy Noname



For 7" masks:


Lyngby 12.07.19
All Layers:
	7" chromium mask
	fracture limits ((-70000, -70000),(70000, 70000))
	Dark periphery
	Chromium down

GDS-file: GLO006_v7.gds
Top cell: wafer

Layer (GDS number): 01 
Mask Type: Digitised data= Dark, right reading
Text(max 30 characters): init-2019-Nitride-etch

Layer (GDS number): 02
Mask Type: Digitised data= Clear, Wrong reading
Text(max 30 characters): init-2019-KOH-backside