| Line 55: | Line 55: | ||
|-style="background:LightGrey; color:black" | |-style="background:LightGrey; color:black" | ||
! Comment | ! Comment | ||
| Tin has not yet been deposited in the Temescal to date ( | | Tin has not yet been deposited in the Temescal to date (May 2022). | ||
Please contact the Thin Film group if you would like us to develop the process. | Please contact the Thin Film group if you would like us to develop the process. | ||
|} | |} | ||
'''*''' ''For thicknesses above 600 nm permission is required.'' | '''*''' ''For thicknesses above 600 nm permission is required.'' | ||