Below are some etched silicon nanostructures with the recipe '''DREM 1kW nano'''
Below are some etched silicon nanostructures with the recipe '''DREM 1kW nano'''
{|
{|
| [[Image:DREM1pic1.jpg |frame|left|x300px|200nm trenches etched with 125 cycles, cross section view]]
| [[Image:DREM1pic1.jpg |frame|x300px|200nm trenches etched with 125 cycles (cross section view)]]
| [[Image:DREM1pic2.jpg |frame|x300px|200nm pillars etched with 100 cycles, cross section view]]
| [[Image:DREM1pic2.jpg |frame|x300px|200nm pillars etched with 100 cycles (cross section view)]]
| [[Image:DREM1pic3.jpg |frame|x300px|200nm pillars etched with 100 cycles, tilted view]]
| [[Image:DREM1pic3.jpg |frame|x300px|200nm pillars etched with 100 cycles (tilted view)]]
|}
|}


Below are some etched silicon nanostructures with the recipe '''DREM 0.5kW nano'''