==Dope with boron==
==Dope with boron==
The furnace A2 boron predep can be used to predeposit silicon wafers with boron. The silicon wafers are positioned in a silicon carbide boat just next to wafers of boron nitride. Boron is predeposited on the silicon wafers. -Rune, hvad er det der sker?
The furnace A2 boron predep can be used to predeposit silicon wafers with boron. The silicon wafers are positioned in a silicon carbide boat just next to wafers of boron nitride. Boron is predeposited on the silicon wafers. '''-Rune, hvad er det der sker?'''


The concentration of boron in the wafer depends on the process temperature.
The concentration of boron in the wafer depends on the process temperature.

Revision as of 08:32, 29 April 2008

Dope with boron

The furnace A2 boron predep can be used to predeposit silicon wafers with boron. The silicon wafers are positioned in a silicon carbide boat just next to wafers of boron nitride. Boron is predeposited on the silicon wafers. -Rune, hvad er det der sker?

The concentration of boron in the wafer depends on the process temperature. The depth profile depends of the process time.

<gallery caption="Boron profiles from SIMS " widths="200px" heights="200px" perrow="3"> image:borDiffusionDepthtable.jpg image:borDiffusionDepthplot.jpg