Specific Process Knowledge/Lithography/EBeamLithography/RaithElphyManual: Difference between revisions
Line 15: | Line 15: | ||
= Mounting of chips or wafers into chamber = | = Mounting of chips or wafers into chamber = | ||
{| cellpadding="2" style="border: 2px solid darkgray;" align="right" | |||
! width="400" | | |||
|- border="0" | |||
| [[File:IMG_0239.jpg|150px]] [[File:IMG_6675.jpg|400px]] | |||
|- align="center" | |||
| Chip holder to Raith Elphy E-beam writer system; the holder has three clamps to hold up to 3 chips and a Faraday's cup to measure beam current. | |||
|} |
Revision as of 20:36, 29 September 2015
Feedback to this page: click here
Purpose, location and technical specifications
The Raith Elphy system is a pattern generator built onto the LEO Scanning Electron Microscope (SEM) in cleanroom F-2. All users must therefore acquire license to use the SEM LEO before acquiring license to the Raith Elphy system.
Techical Specification
The system can be characterized as follows:
- Electron-beam scanning speeds, f, up to X MHz are available (which is maximum scan speed).
- The acceleration voltage is maximum 25 kV.
- The maximum field-size without stitching is X µm x Y µm.
- The machine has a chip holder that fits to 2 - 3 chips with sizes of approximately 1 x 1 cm2 each. A larger chip or wafer can also be mounted on a holder without a Faraday's cup.
Mounting of chips or wafers into chamber
![]() ![]() |
Chip holder to Raith Elphy E-beam writer system; the holder has three clamps to hold up to 3 chips and a Faraday's cup to measure beam current. |