Specific Process Knowledge/Lithography/Baking: Difference between revisions
Appearance
| Line 56: | Line 56: | ||
Maximum 300°C | Maximum 300°C | ||
| | | | ||
Fixed 90°C | Fixed at 90°C | ||
| | | | ||
120 - 250°C | 120 - 250°C | ||
| Line 62: | Line 62: | ||
Return to 120°C after use | Return to 120°C after use | ||
| | | | ||
Fixed 250°C | Fixed at 250°C | ||
|- | |- | ||