At Danchip we have three furnaces and an RTP for annealing: C1, C3, Noble furnace and Jipelec RTP. Annealing normally takes place in an N<sub>2</sub> atmosphere. PECVD PBSG is annealed in an wet atmosphere which will also oxidize the silicon substrate.  
At Danchip we have three furnaces and an RTP for annealing: C1, C3, Noble furnace and Jipelec RTP. Annealing normally takes place in an N<sub>2</sub> atmosphere. PECVD PBSG is annealed in an wet atmosphere which will also oxidize the silicon substrate.  


The furnace for oxidation are made so a 20 minutes N<sub>2</sub> annealing step is include and it is not necessary to make one more.
The furnace for oxidation are made so a 20 minutes N<sub>2</sub> annealing step is include and it is not normally necessary to make one more annealing of the wafers.