Specific Process Knowledge/Thin film deposition/Deposition of Gold: Difference between revisions

From LabAdviser
Knil (talk | contribs)
No edit summary
Knil (talk | contribs)
No edit summary
Line 48: Line 48:
|-style="background:LightGrey; color:black"
|-style="background:LightGrey; color:black"
| Deposition rate
| Deposition rate
|2 Å/s to 15 Å/s
|2 Å/s to 10 Å/s
|1 Å/s to 15 Å/s
|1 Å/s to 10 Å/s
|
|
|Not measured
|Not measured

Revision as of 11:25, 5 March 2014

4th Level - Comparison

Feedback to this page: click here

Gold can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.

E-beam evaporation (Alcatel) E-beam evaporation (Wordentec) Sputter (Lesker) Sputter coater Hummer Sputter coater Balzer
Batch size
  • Up to 1x4" wafers
  • smaller pieces
  • 24x2" wafers or
  • 6x4" wafers or
  • 6x6" wafers
  • up to 1x6" wafer
  • 1x4" wafer
  • Several smaller samples
  • 1 large sample (< 4" wafer)
  • Several smaller samples
Pre-clean RF Ar clean RF Ar clean RF Ar clean
Layer thickness 10 Å to 5000Å* 10 Å to 5000Å* 10 Å to
Deposition rate 2 Å/s to 10 Å/s 1 Å/s to 10 Å/s Not measured Not measured

* For thicknesses above 200 nm permission from ThinFilm group (thinfilm@danchip.dtu.dk) is required.

Adhesion of Au on Si

Adhesion of Au layers


Studies of Au deposition processes

Roughness of Au layers - Roughness of Au layers deposited with different equipment and settings