Specific Process Knowledge/Thin film deposition/Wordentec: Difference between revisions
Appearance
No edit summary |
|||
| Line 18: | Line 18: | ||
! Deposition rate [Å/s] | ! Deposition rate [Å/s] | ||
|- | |- | ||
|Titanium (Ti) | |[[Specific Process Knowledge/Thin film deposition/Deposition of Titanium|Titanium (Ti)]] | ||
|10 | |10 | ||
|- | |- | ||
|Chromium (Cr) | |[[Specific Process Knowledge/Thin film deposition/Deposition of Chromium|Chromium (Cr)]] | ||
|10 | |10 | ||
|- | |- | ||
|Aluminium (Al) | |[[Specific Process Knowledge/Thin film deposition/Deposition of Aluminium|Aluminium (Al)]] | ||
|10 | |10 | ||
|- | |- | ||
|Nickel (Ni) | |[[Specific Process Knowledge/Thin film deposition/Deposition of Nickel|Nickel (Ni)]] | ||
|10 | |10 | ||
|- | |- | ||
|Platinum (Pt) | |[[Specific Process Knowledge/Thin film deposition/Deposition of Platinum|Platinum (Pt)]] | ||
|10 | |10 | ||
|- | |- | ||
|Gold (Au) | |[[Specific Process Knowledge/Thin film deposition/Deposition of Gold|Gold (Au)]] | ||
|10 | |10 | ||
|- | |- | ||
|} | |} | ||
===Thermal evaporation materials=== | ===Thermal evaporation materials=== | ||
Revision as of 12:30, 19 December 2007
Wordentec QCL 800

The Wordentec is a machine for:
- Deposition of metal through E-beam deposition
- Deposition of metal through thermal evaporation
- Deposition of materials through DC sputtering
- Cleaning of samples before deposition through Argon RF sputter clean
The Wordentec is designed to deposit on 1-6 samples in sequence, samples of a size up to 6" in diameter. Adaptors exist for deposition on 2", 4" and 6" wafers, but deposition is possible on samples of almost any size and shape, as long as they do not exceed the size of a 6" substrate. The Wordentec supports either single sample deposition on each sample or batch deposition on six wafers in sequence. It is possible to freely combine processes from the machines different sources.
Process information
The metals available for E-beam evaporation and their standard deposition rates are:
| Metal | Deposition rate [Å/s] |
|---|---|
| Titanium (Ti) | 10 |
| Chromium (Cr) | 10 |
| Aluminium (Al) | 10 |
| Nickel (Ni) | 10 |
| Platinum (Pt) | 10 |
| Gold (Au) | 10 |
Thermal evaporation materials
We currently only have Al available to deposit through thermal evaporation
Sputter materials
It is possible to sputter deposit almost any material, provided that it is possible to deposit with DC sputtering. The materials available currently are:
- TiW alloy (10%/90% by weight)
- Aluminium (Al)
- Chromium (Cr)
- Titanium (Ti)
Sample materials that are approved for entering the chamber
- Silicon
- Silicon oxides
- Silicon nitrides
- Quartz and pyrex
- Metals
- Photoresist
- PMMA
- SU-8
- Mylar