Specific Process Knowledge/Thin film deposition/Deposition of Nickel: Difference between revisions

From LabAdviser
New page: Nickel can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment. {| border="1" cellspacing="0" cellpadding="4" ! ! E-beam evaporati...
 
BGE (talk | contribs)
No edit summary
Line 4: Line 4:
{| border="1" cellspacing="0" cellpadding="4"  
{| border="1" cellspacing="0" cellpadding="4"  
!  
!  
! E-beam evaporation (Alcatel)
! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Alcatel|Alcatel]])
! E-beam evaporation (Leybold)
! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Leybold|Leybold]])
! E-beam evaporation (Wordentec)
! E-beam evaporation ([[Specific Process Knowledge/Thin film deposition/Wordentec|Wordentec]])
|-  
|-  
| Batch size
| Batch size

Revision as of 14:36, 5 February 2009

Nickel can be deposited by e-beam evaporation. In the chart below you can compare the different deposition equipment.


E-beam evaporation (Alcatel) E-beam evaporation (Leybold) E-beam evaporation (Wordentec)
Batch size
  • Up to 1x4" wafers
  • smaller pieces
  • 8x4" wafers or
  • 5x6" wafers
  • 24x2" wafers or
  • 6x4" wafers or
  • 6x6" wafers
Pre-clean RF Ar clean Ar ion bombartment RF Ar clean
Layer thickness 10Å to 1µm 10Å to 0.5µm 10Å to 1 µm
Deposition rate 2Å/s to 15Å/s 1Å/s to 5Å/s 10Å/s to 15Å/s