*1 | *1.5µm resist use the recipe: Danchip_1.5um_4"and6" | ||
*2 | *2.2µm resist use the recipe: Danchip2_2_4" | ||
Please see the parameters for these recipes and some other suggestions in this document:[[media:KS Spinner_thin_resist.xls|Thin resist parameters]] | Please see the parameters for these recipes and some other suggestions in this document:[[media:KS Spinner_thin_resist.xls|Thin resist parameters]] |
Latest revision as of 10:46, 6 March 2008
KS Spinner is the other option for spinning the standard thicknesses.
- 1.5µm resist use the recipe: Danchip_1.5um_4"and6"
- 2.2µm resist use the recipe: Danchip2_2_4"