Template:Spinning KS Spinner: AZ: Difference between revisions
New page: *1,5 um resist use the recipe: Danchip_1,5um_4"and6" *2,2 um resist use the recipe: Danchip2_2_4" Please see the parameters for these recipes and some other suggestions in this document: |
No edit summary |
||
Line 1: | Line 1: | ||
*1,5 um resist use the recipe: Danchip_1,5um_4"and6" | *1,5 um resist use the recipe: Danchip_1,5um_4"and6" | ||
*2,2 um resist use the recipe: Danchip2_2_4" | *2,2 um resist use the recipe: Danchip2_2_4" | ||
Please see the parameters for these recipes and some other suggestions in this document: | Please see the parameters for these recipes and some other suggestions in this document:[[media:KS Spinner_thin_resist.xls|Thin resist parameters]] |
Revision as of 13:57, 1 November 2007
- 1,5 um resist use the recipe: Danchip_1,5um_4"and6"
- 2,2 um resist use the recipe: Danchip2_2_4"
Please see the parameters for these recipes and some other suggestions in this document:Thin resist parameters