Etching at Danchip can be done either with wet chemistry or in dry etch equipment. In general wet chemistry etches isotropically in most materials were as dry etch techniques can be optimized to transfer a given mask pattern with vertical sidewalls (anisotropically) to a given substrate.
Advantages of wet chemistry over dry etch techniques are:
*A often high etch rate difference of different materials giving raise to a high selectivity of the material to be etched compared to underlaying layers or mask materials.
*
== Choose material to be etched ==
== Choose material to be etched ==



Revision as of 16:08, 14 January 2008

Etching at Danchip can be done either with wet chemistry or in dry etch equipment. In general wet chemistry etches isotropically in most materials were as dry etch techniques can be optimized to transfer a given mask pattern with vertical sidewalls (anisotropically) to a given substrate.

Advantages of wet chemistry over dry etch techniques are:

  • A often high etch rate difference of different materials giving raise to a high selectivity of the material to be etched compared to underlaying layers or mask materials.

Choose material to be etched

Choose a dry etch equipment

Choose a wet etch