Specific Process Knowledge/Etch/Etching of Silicon Nitride: Difference between revisions
Appearance
| Line 13: | Line 13: | ||
| | | | ||
*Isotropic etch | *Isotropic etch | ||
* | *Well suited for removing all nitride on a wafer surface (nitride strip) without a mask. High selctivity Si3N4/Si (>100) and Si3N4/SiO2 (>20) @ 180 C. | ||
| | | | ||
*Anisotropic etch: vertical sidewalls | *Anisotropic etch: vertical sidewalls | ||
Revision as of 11:42, 15 November 2007
Silicon nitride can be etched using either wet chemistry or dry etch equipment. Wet chemistry is mainly used to remove all the nitride on the surface (backside and frontside) of a wafer. Dry etching etches one side at a time and can be used to etch structures with several masking materials.
Comparison of wet Silicon Nitride etch and RIE etch for etching of Silicon Nitride
| Wet Silicon Nitride etch | RIE | |
|---|---|---|
| What is it good for: |
|
|
| Possible masking materials: | ? |
|
| Etch rate |
| |
| Process volume |
|
|
| Size of substrate |
|
|