* Open lid @ 110°C:<br />Mean: 109.16°C<br />Uniformity error: 1.12%.
https://labmanager.dtu.dk/view_binary.php?type=data&mach=336
* closed lid @ 110°C:<br />Mean: 109.54°C<br />Uniformity error: 0.89%.


|
|
Line 175: Line 174:
|
|
'''Spincoater: Gamma UV:'''
'''Spincoater: Gamma UV:'''
* TM16 @ 110°C:<br />Mean: 110.1°C<br />Uniformity error: 0.23%.
* TM15 @ 100°C:<br />Mean: 99.5°C<br />Uniformity error: 0.95%.
* TM14 @ 90°C:<br />Mean: 88.9°C<br />Uniformity error: 1.01%.
* TM13 @ 110°C:<br />Mean: 108.6°C<br />Uniformity error: 1.45%.




'''Developer: TMAH UV-lithography:'''
'''Developer: TMAH UV-lithography:'''
Coming soon.




'''Spincoater: Süss stepper:'''
'''Spincoater: Süss stepper:'''
* TM16 @ 175°C:<br />Mean: 174.4°C<br />Uniformity error: 0.72%.
* TM15 @ 175C:<br />Mean: 174.9°C<br />Uniformity error: 0.15%.
* TM14 @ 130°C:<br />Mean: 129.8°C<br />Uniformity error: 0.23%.
* TM13 @ 130°C:<br />Mean: 129.7°C<br />Uniformity error: 0.20%.
* TM12 @ 23°C:<br />Mean: 22.9°C<br />Uniformity error: 0.46%.
* TM11 @ 23°C:<br />Mean: 22.8°C<br />Uniformity error: 0.46%.




'''Developer: Stepper:'''
'''Developer: Stepper:'''


* TM14 @ 130°C:<br />Mean: 129.9°C<br />Uniformity error: 0.62%.
* TM13 @ 130°C:<br />Mean: 130.1°C<br />Uniformity error: 0.73%.
* TM11 @ 20°C:<br />Mean: 20.2°C<br />Uniformity error: 0.10%.


|