The FEI AFEG 250 FEG is a field emission  
The FEI AFEG 250 FEG is a field emission scanning electron microscope with a spatial resolution of 2 nm for the ETD detector in high vacuum at 30 keV. The microscope can operate in high vacuum or low vacuum at room temperature. Our AFEG is fitted with EDS and WDS detectors, which allows for analytical measurements.
scanning electron microscope with a spatial resolution of 2 nm for the ETD detector in high vacuum at 30 keV. The microscope can operate in several modes, such as high vacuum, low vacuum at room temperature. Our AFEG is fitted with EDS and WDS detectors, which allows for analytical measurements in all the operation modes


== Process information ==
== Process information ==
Line 18: Line 17:
Everhart-Thornley (SE/BSE), Solid State BSE, Large Field, Gaseous SE, Gaseous BSE, Gaseous Analytical, STEM, vCD and CCD Camera
Everhart-Thornley (SE/BSE), Solid State BSE, Large Field, Gaseous SE, Gaseous BSE, Gaseous Analytical, STEM, vCD and CCD Camera
*'''Imaging modes'''
*'''Imaging modes'''
High and low vacuum 130 Pa.
High and low vacuum (130 Pa).
*'''Analytical capabilities'''
*'''Analytical capabilities'''
Energy dispersive X-rays (Oxford Instruments 80 mm2 X-Max silicon drift detector, MnKα resolution at 124 eV)
Energy dispersive X-rays (Oxford Instruments 50 mm2 X-Max silicon drift detector, MnKα resolution at 124 eV)
Wave Dispersive Spectrometer
Wave Dispersive Spectrometer



Revision as of 09:02, 16 March 2020

Feedback to this page: click here


The FEI AFEG 250 FEG is a field emission scanning electron microscope with a spatial resolution of 2 nm for the ETD detector in high vacuum at 30 keV. The microscope can operate in high vacuum or low vacuum at room temperature. Our AFEG is fitted with EDS and WDS detectors, which allows for analytical measurements.

Process information

  • Electron source

Field emission gun

  • Accelerating voltage

500 V- 30 kV

  • Resolution

2 nm at 30 kV (SE)

  • Imaging detectors

Everhart-Thornley (SE/BSE), Solid State BSE, Large Field, Gaseous SE, Gaseous BSE, Gaseous Analytical, STEM, vCD and CCD Camera

  • Imaging modes

High and low vacuum (130 Pa).

  • Analytical capabilities

Energy dispersive X-rays (Oxford Instruments 50 mm2 X-Max silicon drift detector, MnKα resolution at 124 eV) Wave Dispersive Spectrometer


Equipment performance and process related parameters

Equipment FEI QFEG 200 Cryo ESEM
Purpose Vizualization and Microanalysis
  • Vizualization of surfaces (topography and Z contrast)
  • Vizualization of projected image (BF STEM image)
  • Energy Dispersive X-ray analysis
Performance Resolution The resolution of QFEG dependends on the sample and the operation mode!
  • 2 nm at 30 keV for Au on C sample with the ETD detector
Instrument specifics Detectors
  • ETD- Everhart-Thornley for secondary electrons
  • BSD- Solid state Back Scattered Detector
  • LFD- Large Field Detector for secondary electrons
  • GSED- Gaseous Secondary Electron Detector
  • GBSD- Gaseous Backscattered Electron Detector
  • GAD- Gaseous Analystical Detector
  • STEM- right field Scanning Tramission Electron detector
  • vCD- low voltage BSED
  • CCD camera
Electron source
  • Field Emission - Tungsten filament
Stage (room temperature)
  • X, Y: 25 × 25 mm
  • T: 0 to 60o (Full tilt require removment of cryo cold trap.)
  • R: 360o
Peltier stage
  • FEI Peltier stage -10o to 22o
Cryo stage
  • Quorum PP2000 Cryo System
EDS
  • Oxford Instruments 80 mm2 X-Max silicon drift detector, MnKα resolution at 124 eV
Operating pressures
  • High vacuum (10-4 Pa), Low vacuum and Enviromental mode (up to 2700Pa)
Substrates Sample sizes
  • No actual limit (limitted by stage movment and detector position).
Allowed materials
  • Conductors, Semiconductors,Insulators,Wet Samples, Biological (not pathogents!)