Specific Process Knowledge/Thin film deposition/DiamondCVD: Difference between revisions
No edit summary |
|||
Line 2: | Line 2: | ||
== SEKI Diamond CVD == | == SEKI Diamond CVD == | ||
The SEKI AX5250S is Microwave Plasma Chemical Vapor Deposition (MPCVD) chamber for growth of diamond thin films. The system is fitted with gasses for diamond growth, which is hydrogen, methane, and oxygen. Depending on your starting material both polycrystalline and single crystalline diamond can be grown. Diamond has a lattice constant of 3.567 Å, which is not easily match to other materials, and therefore in general diamond growth must be seeded by diamond as nucleation sides. For single crystalline diamond this means that diamond layers in most cases must be grown on top of single crystal diamonds. For polycrystalline diamond, almost any material (which can handle 800 °C) will do. It just needs to be seeded with nano diamonds. The seeding can happen by immersion into solution, by polishing, or by spray coating with nano diamonds. | |||
'''The user manual(s), user APV(s), technical information, and contact information can be found in LabManager:''' | '''The user manual(s), user APV(s), technical information, and contact information can be found in LabManager:''' |
Revision as of 12:22, 30 November 2018
Feedback to this page: click here
SEKI Diamond CVD
The SEKI AX5250S is Microwave Plasma Chemical Vapor Deposition (MPCVD) chamber for growth of diamond thin films. The system is fitted with gasses for diamond growth, which is hydrogen, methane, and oxygen. Depending on your starting material both polycrystalline and single crystalline diamond can be grown. Diamond has a lattice constant of 3.567 Å, which is not easily match to other materials, and therefore in general diamond growth must be seeded by diamond as nucleation sides. For single crystalline diamond this means that diamond layers in most cases must be grown on top of single crystal diamonds. For polycrystalline diamond, almost any material (which can handle 800 °C) will do. It just needs to be seeded with nano diamonds. The seeding can happen by immersion into solution, by polishing, or by spray coating with nano diamonds.
The user manual(s), user APV(s), technical information, and contact information can be found in LabManager:
Process information
Software for analysis
Equipment | SEKI AX5250S | |
---|---|---|
Purpose | Diamond growth |
|
Parameters |
H2 |
1000 sccm |
CH4 |
50 sccm | |
O2 |
20 sccm | |
Operating pressure |
>200 Torr | |
Power |
5000 W | |
Temperature |
700-900 °C | |
Substrates | Substrate size |
up to 100 mm wafers, 50 mm prefered |
Allowed materials |
Ask |