Specific Process Knowledge/Etch/ICP Metal Etcher/silicon/isotropic: Difference between revisions
Appearance
No edit summary |
|||
| Line 1: | Line 1: | ||
= Isotropic etching in silicon on the ICP Metal Etch = | = Isotropic etching in silicon on the ICP Metal Etch = | ||
<!--Checked for updates on 11/2-2019 - ok/jmli --> | |||
Revision as of 11:33, 11 February 2019
Isotropic etching in silicon on the ICP Metal Etch
| Recipe | Step | Temp. | Time | Pres. | Hardware | Gasses | RF powers | Observations | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| SF6 | O2 | C4F8 | Ar | CF4 | H2 | CH4 | BCl3 | Cl2 | HBr | Coil | Platen | SEM images of different runs | Keywords | ||||||
| isoslow1 | A | 20 | - | 90 | - | 50 | 0 | 0 | 0 | 0 | 0 | 0 | 0 | 0 | 0 | 400 | 3 | Click HERE! | NA |