'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/AOE_(Advanced_Oxide_Etch)/Silicon_Nitride_Etch_using_AOE/Nitride_etch_with_DUV_mask click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/AOE_(Advanced_Oxide_Etch)/Silicon_Nitride_Etch_using_AOE/Nitride_etch_with_DUV_mask click here]''' | ||
==Silicon nitride etch with STS recommended silicon nitride recipe== | |||
Revision as of 16:05, 15 March 2016
Feedback to this page: click here
Silicon nitride etch with STS recommended silicon nitride recipe
Silicon nitride etch with the standard silicon oxide etch
-
Profile of lines with 1µm pitch
-
Profile of lines with 4µm pitch
-
Profile of 2µm line - zoom in on 4µm pitch