Lyngby 20.06.17 All Layers: 5" chromium mask Soda-lime Glass Dark periphery Chromium down CIF-file: MyMask.cif (or MyMask.gds) Top cell: Wafer (usually) Layer: MT1 Mask Type: Clear field, Right reading Text: DTU PicoTech - Nancy Noname - jun 2015 - Front side mask Layer: MT2 Mask Type: Dark field, Wrong reading Text: DTU PicoTech - Nancy Noname - jun 2015 - Back side mask Yours sincerely Nancy Noname