Specific Process Knowledge/Etch/AOE (Advanced Oxide Etch)/Silicon Nitride Etch using AOE/Nitride etch with DUV mask: Difference between revisions
No edit summary |
|||
Line 2: | Line 2: | ||
===Silicon nitride etch with the standard silicon oxide etch=== | |||
<gallery caption="Etch of LPCVD nitride with DUV KRF resist as mask. The mask is still on. Made by BGHE February 2015 " widths="300px" heights="250px" perrow="3"> | <gallery caption="Etch of LPCVD nitride with DUV KRF resist as mask. The mask is still on. Made by BGHE February 2015 " widths="300px" heights="250px" perrow="3"> |
Revision as of 16:04, 15 March 2016
Feedback to this page: click here
Silicon nitride etch with the standard silicon oxide etch
-
Profile of lines with 1µm pitch
-
Profile of lines with 4µm pitch
-
Profile of 2µm line - zoom in on 4µm pitch