Specific Process Knowledge/Lithography/EBeamLithography/RaithElphyManual: Difference between revisions

From LabAdviser
Tigre (talk | contribs)
Tigre (talk | contribs)
Line 17: Line 17:


# Ventilate the SEM chamber
# Ventilate the SEM chamber
# Mount your chips(s)
# Mount your chips(s) on the Raith Specimen holder
# Mount the holder on the SEM stage, evacuate the SEM chamber


{| cellpadding="2" style="border: 2px solid darkgray;" align="right"
{| cellpadding="2" style="border: 2px solid darkgray;" align="right"
Line 23: Line 24:
|- border="0"
|- border="0"
|[[File:IMG_0239.jpg | 150px]]
|[[File:IMG_0239.jpg | 150px]]
| Chip holder to Raith Elphy E-beam writer system; the holder has three clamps to hold up to 3 chips and a Faraday's cup to measure beam current.
| Chip holder to Raith Elphy E-beam writer system; the holder has three clamps to hold up to 3 chips and a Faraday's cup to measure beam current. The holder is equipped with a dovetail that fits to the stage of the SEM.
|}
|}



Revision as of 20:45, 29 September 2015

Feedback to this page: click here

Purpose, location and technical specifications

The Raith Elphy system is a pattern generator built onto the LEO Scanning Electron Microscope (SEM) in cleanroom F-2. All users must therefore acquire license to use the SEM LEO before acquiring license to the Raith Elphy system.

Techical Specification

The system can be characterized as follows:

  • Electron-beam scanning speeds, f, up to X MHz are available (which is maximum scan speed).
  • The acceleration voltage is maximum 25 kV.
  • The maximum field-size without stitching is X µm x Y µm.
  • The machine has a chip holder that fits to 2 - 3 chips with sizes of approximately 1 x 1 cm2 each. A larger chip or wafer can also be mounted on a holder without a Faraday's cup.

Mounting of chips or wafers into chamber

  1. Ventilate the SEM chamber
  2. Mount your chips(s) on the Raith Specimen holder
  3. Mount the holder on the SEM stage, evacuate the SEM chamber
Chip holder to Raith Elphy E-beam writer system; the holder has three clamps to hold up to 3 chips and a Faraday's cup to measure beam current. The holder is equipped with a dovetail that fits to the stage of the SEM.