Specific Process Knowledge/Lithography/EBeamLithography/RaithElphyManual: Difference between revisions

From LabAdviser
Jump to navigation Jump to search
Line 20: Line 20:


{| cellpadding="2" style="border: 2px solid darkgray;" align="right"
{| cellpadding="2" style="border: 2px solid darkgray;" align="right"
! width="150" |  
! width="150px" |
|- border="0"
|- border="0"
| [[File:IMG_0239.jpg]]
| [[File:IMG_0239.jpg | 150px]]
|- align="center"
|- align="center"
| Chip holder to Raith Elphy E-beam writer system; the holder has three clamps to hold up to 3 chips and a Faraday's cup to measure beam current.
| Chip holder to Raith Elphy E-beam writer system; the holder has three clamps to hold up to 3 chips and a Faraday's cup to measure beam current.
|}
|}

Revision as of 20:41, 29 September 2015

Feedback to this page: click here

Purpose, location and technical specifications

The Raith Elphy system is a pattern generator built onto the LEO Scanning Electron Microscope (SEM) in cleanroom F-2. All users must therefore acquire license to use the SEM LEO before acquiring license to the Raith Elphy system.

Techical Specification

The system can be characterized as follows:

  • Electron-beam scanning speeds, f, up to X MHz are available (which is maximum scan speed).
  • The acceleration voltage is maximum 25 kV.
  • The maximum field-size without stitching is X µm x Y µm.
  • The machine has a chip holder that fits to 2 - 3 chips with sizes of approximately 1 x 1 cm2 each. A larger chip or wafer can also be mounted on a holder without a Faraday's cup.

Mounting of chips or wafers into chamber

  1. Ventilate the SEM chamber
  2. Mount your chips(s)
IMG 0239.jpg
Chip holder to Raith Elphy E-beam writer system; the holder has three clamps to hold up to 3 chips and a Faraday's cup to measure beam current.