LabAdviser/Introduction to LabAdviser and Processing: Difference between revisions
No edit summary |
No edit summary |
||
Line 5: | Line 5: | ||
=Introduction to LabAdviser= | =Introduction to LabAdviser= | ||
[[image:LabAdviser structure.jpg|600px|thumb|]] | [[image:LabAdviser structure.jpg|600px|thumb|]] | ||
LabAdviser is a process handbook for equipment and processes at the DTU Danchip cleanroom | LabAdviser is a process handbook for equipment and processes at the DTU Danchip cleanroom facility and the DTU CEN facility. For the DTU Danchip part, LabAdviser is meant to advise you to a good starting point for your cleanroom process for you to further optimization to meet your needs. | ||
The structure of LabAdviser is designed to guide the users to find the process information they need. The idea is that the user knows what process step is needed. For example if a gold deposit is needed on a 100mm wafer. The user goes to: Main page -> Specific Process Knowledge -> Thin Film Deposition -> Gold. Then the user comes to an overview page describing how to deposit gold at Danchip. From there the user decides whether to use the Alcatel, Wordentec or Sputter System Lesker to do it and get the available process information on the chosen equipment. This example is illustrated in the image to the right. | The structure of LabAdviser is designed to guide the users to find the process information they need. The idea is that the user knows what process step is needed. For example if a gold deposit is needed on a 100mm wafer. The user goes to: Main page -> Specific Process Knowledge -> Thin Film Deposition -> Gold. Then the user comes to an overview page describing how to deposit gold at Danchip. From there the user decides whether to use the Alcatel, Wordentec or Sputter System Lesker to do it and get the available process information on the chosen equipment. This example is illustrated in the image to the right. | ||
Line 12: | Line 12: | ||
*What process step do I need to apply to my sample? <br/> | *What process step do I need to apply to my sample? <br/> | ||
*How can I apply this step to my sample at DTU Danchip? <br/> | *How can I apply this step to my sample at DTU Danchip? <br/> | ||
On the front page there is also a process guide that can help you to overview the content of process page for DTU Danchip and guide you to the relevant page.[[LabAdviser#Overview of processing steps - a guide to where you can find process information in LabAdviser:| Process Guide]] | |||
To view a larger image click [[media:LabAdviser structure.jpg|here]] | To view a larger image click [[media:LabAdviser structure.jpg|here]] |
Revision as of 14:25, 27 January 2016
Feedback to this page: click here
Introduction to LabAdviser

LabAdviser is a process handbook for equipment and processes at the DTU Danchip cleanroom facility and the DTU CEN facility. For the DTU Danchip part, LabAdviser is meant to advise you to a good starting point for your cleanroom process for you to further optimization to meet your needs.
The structure of LabAdviser is designed to guide the users to find the process information they need. The idea is that the user knows what process step is needed. For example if a gold deposit is needed on a 100mm wafer. The user goes to: Main page -> Specific Process Knowledge -> Thin Film Deposition -> Gold. Then the user comes to an overview page describing how to deposit gold at Danchip. From there the user decides whether to use the Alcatel, Wordentec or Sputter System Lesker to do it and get the available process information on the chosen equipment. This example is illustrated in the image to the right.
The image gives an idea of the page tree structure in LabAdviser and also an idea of the thoughts behind the structure. The questions to ask overall are:
- What process step do I need to apply to my sample?
- How can I apply this step to my sample at DTU Danchip?
On the front page there is also a process guide that can help you to overview the content of process page for DTU Danchip and guide you to the relevant page. Process Guide
To view a larger image click here
Introduction to Processing
Take a look at the process example "Solar cell process flow". This is an example of how to build up a process flow for a component you can make at Danchip. Throughout the example you can find links to relevant pages in LabAdviser where information about the different processes are given.