*1,5 um resist use the recipe: Danchip_1,5um_4"and6"
KS Spinner is the other option for spinning the standard thicknesses.
*2,2 um resist use the recipe: Danchip2_2_4"
*1.5µm resist use the recipe: Danchip_1.5um_4"and6"
*2.2µm resist use the recipe: Danchip2_2_4"
Please see the parameters for these recipes and some other suggestions in this document:[[media:KS Spinner_thin_resist.xls|Thin resist parameters]]
Please see the parameters for these recipes and some other suggestions in this document:[[media:KS Spinner_thin_resist.xls|Thin resist parameters]]

Latest revision as of 10:46, 6 March 2008

KS Spinner is the other option for spinning the standard thicknesses.

  • 1.5µm resist use the recipe: Danchip_1.5um_4"and6"
  • 2.2µm resist use the recipe: Danchip2_2_4"

Please see the parameters for these recipes and some other suggestions in this document:Thin resist parameters