Particle counting of an unpatterned surface. A broad range of particles size from 0.1 µm to greater than 3 µm can be measured on a polished silicon or epitaxial layers. Thin films as e.g. Poly-si, Nitride and thermal Oxide can also be inspected. The system will remove small surface roughness so it will not count as particles. | |||
Revision as of 09:41, 13 May 2013
Feedback to this page: click here
KLA-Tencor Surfscan 6420
Particle counting of an unpatterned surface. A broad range of particles size from 0.1 µm to greater than 3 µm can be measured on a polished silicon or epitaxial layers. Thin films as e.g. Poly-si, Nitride and thermal Oxide can also be inspected. The system will remove small surface roughness so it will not count as particles.
Purpose |
| |
---|---|---|
Performance | Particles size |
|
Througput |
| |
Repeatbility |
| |
Process parameter range | Process Temperature |
|
Process pressure |
| |
Substrates | Batch size |
|
Substrate material allowed |