Specific Process Knowledge/Etch/Etching of Platinum: Difference between revisions
Jump to navigation
Jump to search
THIS PAGE IS UNDER CONSTRUCTION
Line 22: | Line 22: | ||
|-style="background:silver; color:black" | |-style="background:silver; color:black" | ||
! | ! | ||
![[Specific Process Knowledge/Etch/Wet | ![[Specific Process Knowledge/Etch/Wet Platinum Etch|Pt wet etch]] | ||
![[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE (Ionfab300+)]] | ![[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300|IBE (Ionfab300+)]] | ||
|- | |- |
Revision as of 11:59, 8 April 2013
THIS PAGE IS UNDER CONSTRUCTION![Under construction.png](/images/thumb/f/f8/Under_construction.png/200px-Under_construction.png.jpeg)
Feedback to this page: click here
Etching of Platinum
Etching of Platinum can be done either by wet etch or by sputtering with ions.
Comparison of Platinum Etch Methods
Pt wet etch | IBE (Ionfab300+) | |
---|---|---|
Generel description | Wet etch of Pt | Sputtering of Pt |
Etch rate range |
|
|
Etch profile |
|
|
Masking material |
|
|
Substrate size |
|
Smaller pieces glued to carrier wafer
|
Allowed materials |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |
|