'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Etching_of_Platin click here]''' | '''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Etching_of_Platin click here]''' | ||
==Etching of | ==Etching of Platinum== | ||
Etching of | Etching of Platinum can be done either by wet etch or by sputtering with ions. | ||
*[[Specific Process Knowledge/Etch/Wet | *[[Specific Process Knowledge/Etch/Wet Platinum Etch|Etching of Platinum by wet etch]] | ||
*[[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300 | *[[Specific_Process_Knowledge/Etch/IBE⁄IBSD Ionfab 300|Sputtering of Pt]] | ||
<br clear="all" /> | <br clear="all" /> | ||
Revision as of 11:33, 8 April 2013
THIS PAGE IS UNDER CONSTRUCTION![Under construction.png](/images/thumb/f/f8/Under_construction.png/200px-Under_construction.png.jpeg)
Feedback to this page: click here
Etching of Platinum
Etching of Platinum can be done either by wet etch or by sputtering with ions.
Comparison of Gold Etch Methods
Au wet etch 1 | Au wet etch 2 | IBE (Ionfab300+) | |
---|---|---|---|
Generel description | Wet etch of Au using Iodine based chemistry | Wet etch of Au using Aqua Regina | Sputtering of Au - pure physical etch |
Etch rate range |
|
|
|
Etch profile |
|
|
|
Masking material |
|
|
|
Substrate size |
|
|
Smaller pieces glued to carrier wafer
|
Allowed materials |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |
No restrictions cross contamination wise as long as you use the right beaker and make sure that they are safe to enter in the chemicals |
|