Feedback to this page: click here
Wet etching of Chromium
Wet etching of chromium at Danchip is done making your own set up in a beaker in a fume hood - preferably in cleanroom 2 or 4. We have two solution for this:
- Commercial chromium etch (Chrome Etch 18)
- HNO3:H2O:cerisulphate - 90ml:1200ml:15g - standard at Danchip
Etch rate are depending on the level of oxidation of the metal.
How to mix the Chromium etch 2:
- Take a beaker and add 15g of cerisulphate.
- Add a little water while stirring - make sure all lumps are gone.
- Add water until 600 ml - keep stirring (use magnetic stirring)
- Add 90 ml HNO3
- When the cerisulphate is completely dissolved (clear liquid) you can add the other 600 ml of wafer.
Overview of the data for the chromium etches
Chromium etch 1 | Chromium etch 2 | ||
---|---|---|---|
General description |
Etch of chromium |
Etch of chromium | |
Link to safety APV and KBA | see APV here. | see APV here | |
Chemical solution | Chrome Etch 18 | HNO3:H2O:cerisulphate - 90ml:1200ml:15g | |
Process temperature | Room temperature | Room Temperature | |
Possible masking materials | Photoresist (1.5 µm AZ5214E) | Photoresist (1.5 µm AZ5214E) | |
Etch rate | . | ~40-100 nm/min | ~? nm/min |
Batch size | 1-7 wafers at a time | 1-7 wafers at a time | |
Size of substrate | 4" wafers | 4" wafers | |
Allowed materials | No restrictions.
Make a note on the beaker of which materials have been processed. |
No restrictions.
Make a note on the beaker of which materials have been processed. |