Etching of Chromium
Etching of chromium can be done either by wet etch, dry etch or by sputtering with ions.
Comparison of Aluminium Etch Metodes
Cr wet etch 1 | Cr wet etch 2 | ICP metal | IBE (Ionfab300+) | |
---|---|---|---|---|
Generel description | Wet etch of Cr that you need to mix your self | Wet etch of Cr premixed | Dry plasma etch of Cr | Sputtering of Cr - pure physical etch |
Etch rate range |
|
|
|
|
Etch profile |
|
|
|
|
Substrate size |
|
|
|
Smaller pieces glued to carrier wafer
|
Allowed materials |
|
|
|
|