Silicon nitride can be etched using either wet chemistry or dry etch equipment. Wet chemistry is mainly used to remove all the nitride on the surface (backside and frontside) of a wafer. Dry etching etches one side at a time and can be used to etch structures with several masking materials.
Comparison of wet Silicon Nitride etch and RIE etch for etching of Silicon Nitride
Wet Silicon Nitride etch | RIE | |
---|---|---|
What is it good for: |
|
|
Possible masking materials: |
|
|
Etch rate |
|
|
Process volume |
|
|
Size of substrate |
|
|