Mask spec: Difference between revisions
New page: ((mask_spec)) |
No edit summary |
||
Line 1: | Line 1: | ||
{{mask_spec}} |
Latest revision as of 15:47, 1 July 2011
For 5" masks: Lyngby 12.07.19 All Layers: 5" chromium mask fracture limits ((-50000, -50000),(50000, 50000)) Dark periphery Chromium down GDS-file: GLO006_v7.gds Top cell: wafer Layer (GDS number): 01 Mask Type: Digitised data= Dark, right reading Text(max 30 characters): init-2019-Nitride-etch Layer (GDS number): 02 Mask Type: Digitised data= Clear, Wrong reading Text(max 30 characters): init-2019-KOH-backside Yours sincerely Nancy Noname For 7" masks: Lyngby 12.07.19 All Layers: 7" chromium mask fracture limits ((-70000, -70000),(70000, 70000)) Dark periphery Chromium down GDS-file: GLO006_v7.gds Top cell: wafer Layer (GDS number): 01 Mask Type: Digitised data= Dark, right reading Text(max 30 characters): init-2019-Nitride-etch Layer (GDS number): 02 Mask Type: Digitised data= Clear, Wrong reading Text(max 30 characters): init-2019-KOH-backside Yours sincerely Nancy Noname