(New page: RIE (Reactive Ion Etch) can be used for etching silicon - both crystalline and polycrystalline silicon. This can be done with a simple photoresist as masking material. The etch can be is...)
 
No edit summary
Line 1: Line 1:
RIE (Reactive Ion Etch) can be used for etching silicon - both crystalline and polycrystalline silicon.   This can be done with a simple photoresist as masking material. The etch can be isotropic or anisotropic with vertical sidewalls depending on the process recipe and the masking material and geometry. The Si is etched by flour radicals that are created from SF<sub>6</sub>(g)in a RF generated plasma.
RIE (Reactive Ion Etch) can be used for etching silicon - both crystalline and polycrystalline silicon.   The etch can be isotropic or anisotropic with vertical sidewalls depending on the process recipe and the masking material and geometry. The Si is etched by flour radicals that are created from SF<sub>6</sub>(g) in a RF generated plasma.
 
===The silicon substrate:===
Most be a wafer of 4" or below or small pieces, not higher than about 2mm.
 
===The silicon can be masked by these materials:===
*Photoresist
*E-beam resist
*Silicon Oxide
*Silicon Nitride
*Aluminium
*Chromium (ONLY RIE2!)
*Other metals if they cover less than 5% of the wafer area (ONLY RIE2!)
 
===Most used recipe (this recipe is being watched in the in the quality assurance program)===

Revision as of 12:04, 8 November 2007

RIE (Reactive Ion Etch) can be used for etching silicon - both crystalline and polycrystalline silicon. The etch can be isotropic or anisotropic with vertical sidewalls depending on the process recipe and the masking material and geometry. The Si is etched by flour radicals that are created from SF6(g) in a RF generated plasma.

The silicon substrate:

Most be a wafer of 4" or below or small pieces, not higher than about 2mm.

The silicon can be masked by these materials:

  • Photoresist
  • E-beam resist
  • Silicon Oxide
  • Silicon Nitride
  • Aluminium
  • Chromium (ONLY RIE2!)
  • Other metals if they cover less than 5% of the wafer area (ONLY RIE2!)

Most used recipe (this recipe is being watched in the in the quality assurance program)