Specific Process Knowledge/Wafer Information: Difference between revisions

From LabAdviser
Kabi (talk | contribs)
Mmat (talk | contribs)
mNo edit summary
 
(27 intermediate revisions by 3 users not shown)
Line 1: Line 1:
{{cc-nanolab}}
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Wafer_Information click here]'''  
'''Feedback to this page''': '''[mailto:labadviser@danchip.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Wafer_Information click here]'''  


== Wafer Information ==
DTU Nanolab has a stock of silicon and glass wafers; the most used of these wafers are located in the wafer cupboard in cleanroom B-1. DTU Danchip seeks always to have new deliveries of wafers on stock. They will be available when the previous delivery has been used.


The wafer box name consists typically of a few letters and a number, eg OP337:
'''All links to Labmanager requires login'''


{| border="1" style="text-align: center; width: 550px; height: 100px;"
== Wafer Information ==
|colspan="3" style="text-align: center;" style="background: #efefef;" | '''waferbox name OP337'''
DTU Nanolab has a stock of standard silicon and glass wafers; the most used of these wafers are located in the wafer cupboard in cleanroom B-1. DTU Nanolab  always try to have new deliveries of wafers on stock. They will be available when the previous delivery has been used.  
|-
!width="30%"|O
!width="35%" |P
!width="35%" |337
|-
|Indicates the company where the wafers are bought
|Type of doping in the wafer
|shipment number
|-
|}
 
 
===How to buy wafers:===
Whenever you want to buy some wafers you login to Labmanager and find the wafer shop [http://labmanager.danchip.dtu.dk/function.php?module=Wafer&view=list&page_id=16| wafer shop]. Here you can see a list of wafers that we have on stock. Most of these are in the cupboard. Some of the wafers are stored in our basement and you must always contact a Nanolab personel for buying these. In the list you can see the specifications, prices as well as a link to a pdf file with more detailed information. Be sure that the wafers you want to buy in the shop are in the cupboard before buying. By buying in the shop the door to the cupboard will unlock for 30 sec and the door can be opened by twisting the handle counter clock wise, leave the door open while taking the wafers you have bought. After taking the number of wafers you have bought place the wafer box back into the cupboard and remember to close the door. This will lock the door again. When taking new wafers always use the dedicated vacuum tweezer hanging on the wall labeled New Wafers.
 
If you buy wafers that have to go directly from the new wafer box into any of the LPCVD furnaces or Furnace C1 buy the numbers of wafers you need minus one. This unlock the door, take the box to the furnace as you close the door to the cupboard behind you, load your wafers into the furnace. Then buy the last wafers for unlocking the cupboard door again such that the wafer box can be placed in the cupboard again.




=== Wafers available in DTU Nanolabs cleanroom ===
=== Wafers available in DTU Nanolabs cleanroom ===


DTU Nanolab
A full list of wafers can be found in the [http://labmanager.danchip.dtu.dk/function.php?module=Wafer&view=shop&page_id=16| wafer shop in Labmanager]. The typical specs of our standard wafers are listet below:
{| border="1" style="text-align: center; width: 550px; height: 100px;"
{| border="1" style="text-align: center; width: 550px; height: 100px;"
|colspan="6" style="text-align: center;" style="background: #efefef;" | '''Wafers available in the cleanroom'''
|colspan="6" style="text-align: center;" style="background: #efefef;" | '''Wafers available in the cleanroom'''
|-
|-
!scope="row" width="15%"| 
!scope="row" width="15%"| 
!width="15%" |Shelf
!width="15%" |Size
!width="15%" |Size
!width="15%" |Type
!width="15%" |Type
Line 41: Line 25:
|-
|-
!SSP (single side polished)
!SSP (single side polished)
|bottom
|2"
|2"
|P
|P
|500 µm
|500 µm
|1-20 Ωcm
|1-20 Ωcm
|-
|-
|-
!SSP (single side polished)
!SSP (single side polished)
|bottom
|4"
|4"
|N+P
|N or P
|525 µm
|525 µm
|1-20 Ωcm
|1-20 Ωcm
|-
|-
!SSP (single side polished)
|6"
|N
|625 µm
|10-20 Ωcm
|-
|-
!SSP (single side polished)
!SSP (single side polished)
|top
|8"
|6"
|N
|725 µm
|1-10 Ωcm
|-
!DSP (double side polished)
|4"
|N or P
|N or P
|625 µm
|350 µm  
|1-20 Ωcm
|1-20 Ωcm
|-
|-
!DSP (double side polished)
|4"
|N
|500 µm
|1-20 Ωcm
|-
|-
!DSP (double side polished)
!DSP (double side polished)
|middle
|6"
|4"
|N
|N+P
|500 µm
|350 µm
|1-20 Ωcm
|1-20 Ωcm
|-
|-
 
!Fused silica wafers
!preprocessed
|4"
|top
| 
|4" and 6"
|500 µm or 1 mm
| 
| 
|-
!Boron glass wafers
|4"
| 
| 
|500 µm
| 
| 
|-
|-
!Boron glasswafers
!pre-processed<sup>{{fn|1}}</sup>
|middle
|4" and 6"
|4"
|&nbsp;
|&nbsp;
|&nbsp;
|1 mm
|&nbsp;
|&nbsp;
|-
|-
|}
|}
<sup>{{fn|1}}</sup> Pre-processed wafers are wafers with various thicknesses or thermal oxides, LPCVD nitrides and Poly Si. Please consult the [http://labmanager.danchip.dtu.dk/function.php?module=Wafer&view=shop&page_id=16| wafer shop in Labmanager]for details.
The name on the wafer boxes consists typically of a few letters and a number, eg OP337:
{| border="1" style="text-align: center; width: 550px; height: 100px;"
|colspan="3" style="text-align: center;" style="background: #efefef;" | '''waferbox name OP337'''
|-
!width="30%"|O
!width="35%" |P
!width="35%" |337
|-
|Indicates the company where the wafers are bought
|Type of doping in the wafer
|shipment number
|-
|}
=== How to buy wafers ===
Whenever you want to buy some wafers you login to Labmanager and find the [http://labmanager.danchip.dtu.dk/function.php?module=Wafer&view=shop&page_id=16| wafer shop in Labmanager]. Here you can see a list of wafers that we have on stock. Most of these are in the cupboard. Some of the wafers are stored in our basement and you must always contact a Nanolab personnel for buying these. In the list you can see the specifications, prices as well as a link to a pdf file with more detailed information. Be sure that the wafers you want to buy in the shop are in the cupboard before buying. By buying in the shop the door to the cupboard will unlock for 30 sec and the door can be opened by twisting the handle counter clock wise, leave the door open while taking the wafers you have bought. After taking the number of wafers you have bought place the wafer box back into the cupboard and remember to close the door. This will lock the door again. When taking new wafers always use the dedicated vacuum tweezer hanging on the wall labeled Wafer Shop Tweezer.
If you buy wafers that have to go directly from the new wafer box into any of the LPCVD furnaces or Furnace: Anneal-oxide(C1) buy the numbers of wafers you need minus one. This unlock the door, take the box to the furnace as you close the door to the cupboard behind you, load your wafers into the furnace. Then buy the last wafer for unlocking the cupboard door such that the wafer box can be placed in the cupboard again.


=== Wafer boxes and single wafer carriers ===
=== Wafer boxes and single wafer carriers ===


New clean wafer boxes and single wafer carriers can be found in the gowning area. Ask DTU Nanolab personnel for help if stock is low.
New clean wafer boxes and single wafer carriers can be found in the gowning area. Ask DTU Nanolab personnel for help if stock is low. If you empty a wafer box from the wafer cupboard you can also keep that, it is considered very clean.

Latest revision as of 15:49, 12 February 2025

The contents on this page, including all images and pictures, was created by DTU Nanolab staff unless otherwise stated.

Feedback to this page: click here


All links to Labmanager requires login

Wafer Information

DTU Nanolab has a stock of standard silicon and glass wafers; the most used of these wafers are located in the wafer cupboard in cleanroom B-1. DTU Nanolab always try to have new deliveries of wafers on stock. They will be available when the previous delivery has been used.


Wafers available in DTU Nanolabs cleanroom

A full list of wafers can be found in the wafer shop in Labmanager. The typical specs of our standard wafers are listet below:

Wafers available in the cleanroom
  Size Type Thickness Resistivity
SSP (single side polished) 2" P 500 µm 1-20 Ωcm
SSP (single side polished) 4" N or P 525 µm 1-20 Ωcm
SSP (single side polished) 6" N 625 µm 10-20 Ωcm
SSP (single side polished) 8" N 725 µm 1-10 Ωcm
DSP (double side polished) 4" N or P 350 µm 1-20 Ωcm
DSP (double side polished) 4" N 500 µm 1-20 Ωcm
DSP (double side polished) 6" N 500 µm 1-20 Ωcm
Fused silica wafers 4"   500 µm or 1 mm  
Boron glass wafers 4"   500 µm  
pre-processed1 4" and 6"      

1 Pre-processed wafers are wafers with various thicknesses or thermal oxides, LPCVD nitrides and Poly Si. Please consult the wafer shop in Labmanagerfor details.


The name on the wafer boxes consists typically of a few letters and a number, eg OP337:

waferbox name OP337
O P 337
Indicates the company where the wafers are bought Type of doping in the wafer shipment number

How to buy wafers

Whenever you want to buy some wafers you login to Labmanager and find the wafer shop in Labmanager. Here you can see a list of wafers that we have on stock. Most of these are in the cupboard. Some of the wafers are stored in our basement and you must always contact a Nanolab personnel for buying these. In the list you can see the specifications, prices as well as a link to a pdf file with more detailed information. Be sure that the wafers you want to buy in the shop are in the cupboard before buying. By buying in the shop the door to the cupboard will unlock for 30 sec and the door can be opened by twisting the handle counter clock wise, leave the door open while taking the wafers you have bought. After taking the number of wafers you have bought place the wafer box back into the cupboard and remember to close the door. This will lock the door again. When taking new wafers always use the dedicated vacuum tweezer hanging on the wall labeled Wafer Shop Tweezer.

If you buy wafers that have to go directly from the new wafer box into any of the LPCVD furnaces or Furnace: Anneal-oxide(C1) buy the numbers of wafers you need minus one. This unlock the door, take the box to the furnace as you close the door to the cupboard behind you, load your wafers into the furnace. Then buy the last wafer for unlocking the cupboard door such that the wafer box can be placed in the cupboard again.

Wafer boxes and single wafer carriers

New clean wafer boxes and single wafer carriers can be found in the gowning area. Ask DTU Nanolab personnel for help if stock is low. If you empty a wafer box from the wafer cupboard you can also keep that, it is considered very clean.