Specific Process Knowledge/Back-end processing/Polishing machine: Difference between revisions

From LabAdviser
Sifkle (talk | contribs)
No edit summary
Jehan (talk | contribs)
No edit summary
 
(9 intermediate revisions by 3 users not shown)
Line 4: Line 4:
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.'''
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.'''


'''All links to Kemibrug (SDS) and Labmanager Including APV and QC requires login.'''
'''All links Labmanager requires login.'''


<big>''' Machine decommissioned end of 2024 '''
</big>
== Polisher/Lapper ==


== Polisher/Lapper ==
<big>''' Machine decommissioned end of 2024 '''
</big>


[[image:Logitech pm5 1.jpg|400px|right|thumb|The Logitech PM5 Polisher/Lapper]]
<!-- copyright issue rkc -->
Training is required before using th machine. The machine is equipped with a LabManager lock.
<!-- copyright issue rkc [[image:Logitech pm5 1.jpg|400px|right|thumb|The Logitech PM5 Polisher/Lapper]]
Training is required before using th machine. The machine is equipped with a LabManager lock.-->


The Logitech PM5 Polisher/Lapper is for thinning down wafers and other substrates.  
The Logitech PM5 Polisher/Lapper is for thinning down wafers and other substrates.  
Line 22: Line 27:
==Equipment performance and process related parameters==
==Equipment performance and process related parameters==


[[File:IMG_20230228_113121.jpg|thumb|350px|PM5 lapper in Fume hood]]
{| border="2" cellspacing="0" cellpadding="2"  
{| border="2" cellspacing="0" cellpadding="2"  


Line 108: Line 114:
*Allowed material 3 -->
*Allowed material 3 -->
|-  
|-  
|}
|}  
[[File:IMG_20230228_113134.jpg|thumb|left|300px|lapping jig]]
[[File:IMG_20230228_113127.jpg|thumb|1000px|mounting/measuring space]]


<br clear="all" />
<br clear="all" />

Latest revision as of 15:02, 30 January 2025

Feedback to this page: click here

Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.

All links Labmanager requires login.

Machine decommissioned end of 2024

Polisher/Lapper

Machine decommissioned end of 2024


The Logitech PM5 Polisher/Lapper is for thinning down wafers and other substrates.

The user manual, user APV, technical information and contact information can be found in LabManager:

The Logitech PM5 Polisher/Lapper in LabManager

Equipment performance and process related parameters

PM5 lapper in Fume hood
Equipment Polisher/Lapper
Purpose

Thinning of substrates of

  • InP
  • GaAs
  • Silicon
  • Metals
  • Glass/Quartz
Performance Thinning
  • Removal rate: 1-10µm/min
  • Thickness accuracy: +/- 10 µm
  • Thickness homogeneity: +/- 10 µm
  • Roughness: +/- ? µm
Polishing
  • Removal rate: ~1 µm/min
  • Thickness accuracy: ? µm
  • Thickness homogeneity: ? µm
  • Roughness: +/- ? µm
Process parameter range Polishing liquid
  • Al2O3 (alumina) powder: 3, 9 or 20 µm
  • Chemlox (for polishing)
  • SF1 Polishing Fluid (for polishing e.g. SiO2)
Polishing cloths
  • Chemcloth Polishing Cloths (for use with SF1 liquid)
Rotation speed
  • Thinning: 5-20 rpm
  • Polishing: 5-80 rpm
Arm sweep
  • Thinning: stationary
  • Polishing: 12% (inner) - 80% (outer)
Substrates Batch size
  • # small samples
  • one 50 mm wafer
  • one 100 mm wafer
Allowed materials
  • InP
  • GaAs
  • Silicon
  • Metals
  • Glass/Quartz
lapping jig