== Polisher/Lapper [[Image:section under construction.jpg|70px]] ==
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.'''


[[image:Logitech pm5 1.jpg|400px|right|thumb|The Logitech PM5 Polisher/Lapper]]
'''All links Labmanager requires login.'''
 
<big>''' Machine decommissioned end of 2024 '''
</big>
== Polisher/Lapper ==
 
<big>''' Machine decommissioned end of 2024 '''
</big>
 
<!-- copyright issue rkc -->
<!-- copyright issue rkc [[image:Logitech pm5 1.jpg|400px|right|thumb|The Logitech PM5 Polisher/Lapper]]
Training is required before using th machine. The machine is equipped with a LabManager lock.-->


The Logitech PM5 Polisher/Lapper is for thinning down wafers and other substrates.  
The Logitech PM5 Polisher/Lapper is for thinning down wafers and other substrates.  


'''The user manual, user APV(s), technical information and contact information can be found in LabManager:'''  
'''The user manual, user APV, technical information and contact information can be found in LabManager:'''  
<!-- remember to remove the type of documents that are not present -->
<!-- remember to remove the type of documents that are not present -->


Line 16: Line 27:
==Equipment performance and process related parameters==
==Equipment performance and process related parameters==


[[File:IMG_20230228_113121.jpg|thumb|350px|PM5 lapper in Fume hood]]
{| border="2" cellspacing="0" cellpadding="2"  
{| border="2" cellspacing="0" cellpadding="2"  


Line 57: Line 69:
*Performance range -->
*Performance range -->
|-
|-
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Process parameter range
!style="background:silver; color:black" align="center" valign="center" rowspan="4"|Process parameter range
|style="background:LightGrey; color:black"|Polishing liquid
|style="background:LightGrey; color:black"|Polishing liquid
|style="background:WhiteSmoke; color:black"|
|style="background:WhiteSmoke; color:black"|
*Al2O3 (alumina) powder: 3, 9 or 20 µm
*Al2O3 (alumina) powder: 3, 9 or 20 µm
*Chemlox (for polishing)
*Chemlox (for polishing)
*SF1 Polishing Fluid (for polishing e.g. SiO2)
|-
|style="background:LightGrey; color:black"|Polishing cloths
|style="background:WhiteSmoke; color:black"|
*Chemcloth Polishing Cloths (for use with SF1 liquid)
|-
|-
|style="background:LightGrey; color:black"|Rotation speed
|style="background:LightGrey; color:black"|Rotation speed
Line 97: Line 114:
*Allowed material 3 -->
*Allowed material 3 -->
|-  
|-  
|}
|}  
[[File:IMG_20230228_113134.jpg|thumb|left|300px|lapping jig]]
[[File:IMG_20230228_113127.jpg|thumb|1000px|mounting/measuring space]]


<br clear="all" />
<br clear="all" />

Latest revision as of 15:02, 30 January 2025

Feedback to this page: click here

Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.

All links Labmanager requires login.

Machine decommissioned end of 2024

Polisher/Lapper

Machine decommissioned end of 2024


The Logitech PM5 Polisher/Lapper is for thinning down wafers and other substrates.

The user manual, user APV, technical information and contact information can be found in LabManager:

The Logitech PM5 Polisher/Lapper in LabManager

Equipment performance and process related parameters

PM5 lapper in Fume hood
Equipment Polisher/Lapper
Purpose

Thinning of substrates of

  • InP
  • GaAs
  • Silicon
  • Metals
  • Glass/Quartz
Performance Thinning
  • Removal rate: 1-10µm/min
  • Thickness accuracy: +/- 10 µm
  • Thickness homogeneity: +/- 10 µm
  • Roughness: +/- ? µm
Polishing
  • Removal rate: ~1 µm/min
  • Thickness accuracy: ? µm
  • Thickness homogeneity: ? µm
  • Roughness: +/- ? µm
Process parameter range Polishing liquid
  • Al2O3 (alumina) powder: 3, 9 or 20 µm
  • Chemlox (for polishing)
  • SF1 Polishing Fluid (for polishing e.g. SiO2)
Polishing cloths
  • Chemcloth Polishing Cloths (for use with SF1 liquid)
Rotation speed
  • Thinning: 5-20 rpm
  • Polishing: 5-80 rpm
Arm sweep
  • Thinning: stationary
  • Polishing: 12% (inner) - 80% (outer)
Substrates Batch size
  • # small samples
  • one 50 mm wafer
  • one 100 mm wafer
Allowed materials
  • InP
  • GaAs
  • Silicon
  • Metals
  • Glass/Quartz
lapping jig
mounting/measuring space