'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/ | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Silicon_Carbide click here]''' | ||
<br clear="all" /> | <br clear="all" /> | ||
Line 5: | Line 5: | ||
== Deposition of Silicon Carbide == | == Deposition of Silicon Carbide == | ||
Silicon Carbide (SiC) can be deposited by RF-sputtering method. So far the process has been tested only using [[Specific Process Knowledge/Thin film deposition/Lesker|Sputter-System (Lesker)]]: | Silicon Carbide (SiC) can be deposited by RF-sputtering method. So far the process has been tested only using [[Specific Process Knowledge/Thin film deposition/Lesker|Sputter-System (Lesker)]] (Src5-RF): | ||
*[[/Deposition of SiC in Sputter-System Lesker|Deposition of SiC in Sputter-System (Lesker)]] | *[[/Deposition of SiC in Sputter-System Lesker|Deposition of SiC in Sputter-System (Lesker)]] |
Latest revision as of 13:44, 9 January 2025
Feedback to this page: click here
Deposition of Silicon Carbide
Silicon Carbide (SiC) can be deposited by RF-sputtering method. So far the process has been tested only using Sputter-System (Lesker) (Src5-RF):