Created page with "'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php?title=Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Scandium_Nitride&action=submit click here]''' <i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i> == Deposition of Niobium Titanium Nitride == Deposition of ScN can only be done by reactive sputtering using Sc target. The on..."
 
Eves (talk | contribs)
No edit summary
 
(3 intermediate revisions by the same user not shown)
Line 3: Line 3:
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i>
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i>


== Deposition of Niobium Titanium Nitride ==
== Deposition of Scandium Nitride ==
   
   
Deposition of ScN can only be done by reactive sputtering using Sc target.
Deposition of ScN can only be done by reactive sputtering using Sc target.
Line 9: Line 9:
The only tool for this application is the Cluster-based multi-chamber high vacuum sputtering deposition system, commonly referred to as the 'Cluster Lesker.' The operating process is thoroughly documented and described in detail.:
The only tool for this application is the Cluster-based multi-chamber high vacuum sputtering deposition system, commonly referred to as the 'Cluster Lesker.' The operating process is thoroughly documented and described in detail.:


* [[Specific Process Knowledge/Thin film deposition/Deposition of Scandium Nitride/ScN Reactive RF Sputtering in Cluster Lesker PC3|Deposition of Scandium Nitride (Sc) using reactive RF sputtering]] in Sputter-System Metal-Nitride(PC3) Source 1 (4-inch target)
* [[Specific Process Knowledge/Thin film deposition/Deposition of Scandium Nitride/ScN Reactive Sputtering in Cluster Lesker PC3|Deposition of Scandium Nitride (ScN) using reactive sputtering]] in Sputter-System Metal-Nitride(PC3) Source 1 (4-inch target)


At the moment (October 2023) we have a 4-inch Sc target (0.250" thick bonded to Cu) for PC3 Src1.
At the moment (October 2023) we have a 4-inch Sc target (0.250" thick, bonded to Cu) for PC3 Src1.

Latest revision as of 13:56, 9 November 2023

Feedback to this page: click here

Unless otherwise stated, this page is written by DTU Nanolab internal

Deposition of Scandium Nitride

Deposition of ScN can only be done by reactive sputtering using Sc target.

The only tool for this application is the Cluster-based multi-chamber high vacuum sputtering deposition system, commonly referred to as the 'Cluster Lesker.' The operating process is thoroughly documented and described in detail.:

At the moment (October 2023) we have a 4-inch Sc target (0.250" thick, bonded to Cu) for PC3 Src1.