Specific Process Knowledge/Etch/DRIE-Pegasus/Pegasus-4/SiO2 Etch/Cr mask: Difference between revisions
Created page with "'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DRIE-Pegasus/Pegasus-4/SiO2_Etch/Cr_mask click here]'''" |
No edit summary |
||
Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DRIE-Pegasus/Pegasus-4/SiO2_Etch/Cr_mask click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/DRIE-Pegasus/Pegasus-4/SiO2_Etch/Cr_mask click here]'''<br> | ||
{{CC-bghe2}} | |||
<gallery caption="EM tests with Cr mask on full wafer 6 min etch" perrow="3" widths="400px" heights="300px"> | |||
File:C09721_center_05.jpg | |||
File:C09721_center_07.jpg | |||
File:C09721_center_10.jpg | |||
File:C09721_center_18.jpg | |||
File:C09721_center_21.jpg | |||
File:C09721_center_22.jpg | |||
</gallery> |
Revision as of 13:40, 21 September 2023
Feedback to this page: click here
Unless otherwise stated, all content in this section was done by Berit Herstrøm, DTU Nanolab