==Looking at bit on the effect of using electromagnets for etching SiO2 with DUV resist== | ==Looking at bit on the effect of using electromagnets for etching SiO2 with DUV resist== | ||
{{CC-bghe2}} | {{CC-bghe2}} | ||
*Removing the H2 from the recipe to get less redeposition |
Revision as of 09:28, 11 September 2023
Looking at bit on the effect of using electromagnets for etching SiO2 with DUV resist
Unless otherwise stated, all content in this section was done by Berit Herstrøm, DTU Nanolab
- Removing the H2 from the recipe to get less redeposition