Specific Process Knowledge/Thin film deposition/DiamondCVD: Difference between revisions
No edit summary |
|||
Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/DiamondCVD click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/DiamondCVD click here]''' | ||
<i> Unless otherwise stated, this page is written by <b>DTU Nanolab internal</b></i> | |||
== SEKI Diamond CVD == | == SEKI Diamond CVD == |
Revision as of 12:55, 6 June 2023
Feedback to this page: click here
Unless otherwise stated, this page is written by DTU Nanolab internal
SEKI Diamond CVD
The SEKI AX5250S is a Microwave Plasma Chemical Vapor Deposition (MPCVD) system for growth of diamond thin films. The system is fitted with hydrogen, methane, and oxygen for diamond growth.
Depending on the starting material both polycrystalline and single crystalline diamond can be grown. Diamond has a lattice constant of 3.567 Å, which is not easily matched to other materials, and therefore in general diamond growth must be seeded by diamond as nucleation sites.
For single crystalline diamond this means that diamond layers in most cases must be grown on top of single crystal diamonds. For polycrystalline diamond, almost any material will do as long as it can withstand a growth temperature of 800 °C. It just needs to be seeded with nano diamonds. The seeding can happen by immersion into solution, by polishing, or by spray coating with nano diamonds.
The user manual, APV, technical information, and contact information can be found in LabManager:
More details
Equipment | SEKI AX5250S | |
---|---|---|
Purpose | Diamond growth |
|
Parameters |
H2 |
Up to 1000 sccm |
CH4 |
Up to 50 sccm | |
O2 |
Up to 20 sccm (may be reduced, check) | |
Operating pressure |
Max. >200 Torr (usually about 120 Torr for diamond growth) | |
Power |
Up to 5000 W | |
Temperature |
700-900 °C | |
Process | Growth rate |
About 8 Å/s (3 μm/hr) |
Max thickness |
About 100 μm | |
Uniformity |
OK up to 50 mm diameter | |
Substrates | Substrate size |
up to 100 mm wafers, 50 mm preferred |
Allowed materials |