'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Alumina click here]''' | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Alumina click here]''' | ||
''All text by Nanolab staff'' | |||
==Deposition of aluminium oxide== | ==Deposition of aluminium oxide== |
Revision as of 15:37, 1 June 2023
Feedback to this page: click here
All text by Nanolab staff
Deposition of aluminium oxide
Aluminium oxide (Alumina, Al2O3) can be deposited by use of ALD (atomic layer deposition) or by sputtering. During the sputter deposition oxygen is added to the chamber resulting in aluminium oxide on the sample.
Comparison of the methods for deposition of Alumium Oxide
Sputter-System(Lesker) | Sputter-System Metal-Oxide(PC1) | ALD Picosun 200 | |
---|---|---|---|
Generel description |
|
|
|
Stoichiometry |
|
|
|
Film Thickness |
|
|
|
Deposition rate |
|
|
|
Step coverage |
|
|
|
Process Temperature |
|
|
|
More info on Al2O3 | |||
Substrate size |
|
|
|
Allowed materials |
|
|
|