Specific Process Knowledge/Wafer cleaning/Post CMP Cleaner: Difference between revisions
No edit summary |
|||
(6 intermediate revisions by 2 users not shown) | |||
Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@ | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.danchip.dtu.dk/index.php/Specific_Process_Knowledge/Wafer_cleaning/Post_CMP_Cleaner click here]''' | ||
'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.''' | |||
'''All links to Labmanager requires login.''' | |||
== Post CMP Cleaner) == | == Post CMP Cleaner) == | ||
[[image: | [[image:post cmp cleaner.jpg|400px|right|thumb|The Post CMP CLeaner in cleanroom A-5]] | ||
The post CMP Cleaner is designed for removing slurry residues from polishing wafers. | The post CMP Cleaner is designed for removing slurry residues from polishing wafers. The Post CMP cleaner is the recommended cleaning tool after using the '''[http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Back-end_processing/Polisher_CMP Polisher CMP]'''. | ||
Line 16: | Line 18: | ||
<!-- give the link to the equipment info page in LabManager: --> | <!-- give the link to the equipment info page in LabManager: --> | ||
[http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=431 The Post CMP Cleaner in LabManager] | [http://labmanager.danchip.dtu.dk/function.php?module=Machine&view=view&mach=431 The Post CMP Cleaner in LabManager] | ||
==Equipment performance and process related parameters== | |||
{| border="2" cellspacing="0" cellpadding="2" | |||
!colspan="2" border="none" style="background:silver; color:black;" align="center"|Equipment | |||
|style="background:WhiteSmoke; color:black"|<b>Post CMP Cleaner</b> | |||
<!-- |style="background:WhiteSmoke; color:black"|<b>Equipment 2</b> --> | |||
|- | |||
!style="background:silver; color:black;" align="center" width="60"|Purpose | |||
|style="background:LightGrey; color:black"| | |||
Cleaning of | |||
|style="background:WhiteSmoke; color:black"| | |||
*Samples from the CMP | |||
<!-- |style="background:WhiteSmoke; color:black"| | |||
*Purpose 1 | |||
*Purpose 2 | |||
*Purpose 3 --> | |||
|- | |||
|- | |||
!style="background:silver; color:black" align="center" valign="center" rowspan="4"|Process parameter range | |||
|- | |||
|style="background:LightGrey; color:black"|Mechanical Cleaning | |||
|style="background:WhiteSmoke; color:black"| | |||
*Brush Cleaning | |||
|- | |||
|style="background:LightGrey; color:black"|Power | |||
|style="background:WhiteSmoke; color:black"| | |||
*Megasonic Power from 0-40 W (in water) | |||
|- | |||
|style="background:LightGrey; color:black"|Arm sweep | |||
|style="background:WhiteSmoke; color:black"| | |||
*4" and 6" (20x20mm and 2" run with a 4" sweep) | |||
|- | |||
!style="background:silver; color:black" align="center" valign="center" rowspan="3"|Substrates | |||
|style="background:LightGrey; color:black"|Sample size | |||
|style="background:WhiteSmoke; color:black"| | |||
*<nowiki></nowiki> one 20x20mm piece | |||
*one 50 mm wafer | |||
*one 2" wafer | |||
*one 100 mm wafer | |||
*one 150 mm wafer | |||
<!-- |style="background:WhiteSmoke; color:black"| | |||
*<nowiki>#</nowiki> small samples | |||
*<nowiki>#</nowiki> 50 mm wafers | |||
*<nowiki>#</nowiki> 100 mm wafers | |||
*<nowiki>#</nowiki> 150 mm wafers --> | |||
|- | |||
| style="background:LightGrey; color:black"|Allowed materials | |||
|style="background:WhiteSmoke; color:black"| | |||
*Silicon | |||
*Polysilicon | |||
*Silicon Oxide | |||
*Glass/Quartz | |||
<!-- |style="background:WhiteSmoke; color:black"| | |||
*Allowed material 1 | |||
*Allowed material 2 | |||
*Allowed material 3 --> | |||
|- | |||
|} | |||
<br clear="all" /> |
Latest revision as of 13:57, 13 February 2023
Feedback to this page: click here
Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.
All links to Labmanager requires login.
Post CMP Cleaner)

The post CMP Cleaner is designed for removing slurry residues from polishing wafers. The Post CMP cleaner is the recommended cleaning tool after using the Polisher CMP.
The user manual, user APV, technical information and contact information can be found in LabManager:
The Post CMP Cleaner in LabManager
Equipment | Post CMP Cleaner | |
---|---|---|
Purpose |
Cleaning of |
|
Process parameter range | ||
Mechanical Cleaning |
| |
Power |
| |
Arm sweep |
| |
Substrates | Sample size |
|
Allowed materials |
|