Specific Process Knowledge/Etch/IBE⁄IBSD Ionfab 300/SIMS settings: Difference between revisions
Created page with "{| border="1" style="text-align: center; width: 320px; height: 200px;" |- |colspan="3" style="text-align: center;" style="background: #efefef;" | '''IBSD setting for differen..." |
No edit summary |
||
(6 intermediate revisions by the same user not shown) | |||
Line 1: | Line 1: | ||
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/IBE⁄IBSD_Ionfab_300/SIMS_settings click here]''' | |||
<br> {{CC-bghe1}} - ''2015''<br> | |||
{| border="1" style="text-align: center; width: 320px; height: 200px;" | {| border="1" style="text-align: center; width: 320px; height: 200px;" | ||
|- | |- | ||
|colspan="3" style="text-align: center;" style="background: | |colspan="3" style="text-align: center;" style="background:Black; color:White;" | '''SIMS setting for different materials''' | ||
|- | |- |
Latest revision as of 16:50, 6 February 2023
Feedback to this page: click here
This page is written by Berit Herstrøm @ DTU Nanolab (BGHE) if nothing else is stated - 2015
SIMS setting for different materials | ||
Lower plate | Upper plate | |
---|---|---|
Ti | -1 | |
Si | -1 | (2) |
Al | -1 | 1 |
Cr | -1 | |
Ni | -6 |