= Techniques, hardware and challenges common to all dry etch tools = | = Techniques, hardware and challenges common to all dry etch tools = | ||
This page contains information that is common to dry etch instruments. | This page contains information that is common to dry etch instruments. | ||
{| border ="0" align="left" valign="top" | {| border ="0" align="left" valign="top" | ||
Line 14: | Line 13: | ||
| style="background:#DCDCDC;"| Comparison of the different hardware setups | | style="background:#DCDCDC;"| Comparison of the different hardware setups | ||
|- | |- | ||
| style="background: LightGray"| [[/Bonding| | | style="background: LightGray"| [[/Bonding| Using carrier wafer]] | ||
| style="background: #DCDCDC"| Processing different sizes of substrates by bonding | | style="background: #DCDCDC"| Processing different sizes of substrates by using a carriers: bonding or not bonding | ||
|- | |- | ||
| style="background: LightGray"| [[/OES| Optical Endpoint System]] | | style="background: LightGray"| [[/OES| Optical Endpoint System]] | ||
| style="background: #DCDCDC"| Using the OES technique to find endpoints and to diagnose plasmas | | style="background: #DCDCDC"| Using the OES technique to find endpoints and to diagnose plasmas | ||
|- | |- | ||
| style="background: LightGray"| [[/LEP| LASER Endpoint System]] | |||
| style="background: #DCDCDC"| Using the LEP technique to find endpoints between interfaces or at a etch depth (in transparent layers) | |||
|- | |||
| style="background: LightGray"| [[/Data4dryetch| Etch product volatility]] | |||
| style="background: #DCDCDC"| Links to various tables with data on etch product volatility | |||
|- | |||
|} | |} |
Latest revision as of 12:50, 3 February 2023
Feedback to this page: click here
Techniques, hardware and challenges common to all dry etch tools
This page contains information that is common to dry etch instruments.
Dry etch page | Description |
---|---|
Hardware comparison | Comparison of the different hardware setups |
Using carrier wafer | Processing different sizes of substrates by using a carriers: bonding or not bonding |
Optical Endpoint System | Using the OES technique to find endpoints and to diagnose plasmas |
LASER Endpoint System | Using the LEP technique to find endpoints between interfaces or at a etch depth (in transparent layers) |
Etch product volatility | Links to various tables with data on etch product volatility |