'''Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.'''
== Laser sources ==  
== Laser sources ==  


The laser micromachining tool is equipped with  two laser sources (1) a picosecond laser (TBW) and (2) a nanosecond laser (IPG). The technical specifications provided by the supplier 3D micromac are shown below. Refer to the [[Specific_Process_Knowledge/Back-end_processing/Laser_Micromachining_Tool#Performances/|Performances]] to know the measured values.  
The laser micromachining tool is equipped with  two laser sources (1) a picosecond laser (TBW) and (2) a nanosecond laser (IPG). The technical specifications provided by the supplier 3D micromac are shown below. Refer to the [[Specific_Process_Knowledge/Back-end_processing/Laser_Micromachining_Tool#Performances/|Performances]] to know the measured values of the output power. From 1st of Mar 2017 only the pico second laser is available \ rkch.


=== Specifications from 3D micromac ===  
=== Specifications from 3D micromac ===  
Line 17: Line 20:
|style="background:LightGrey; color:black"|Pulse duration
|style="background:LightGrey; color:black"|Pulse duration
|style="background:WhiteSmoke; color:black"| 10ps
|style="background:WhiteSmoke; color:black"| 10ps
|style="background:WhiteSmoke; color:black"| 120ns
|style="background:WhiteSmoke; color:black"| 100ns
|-
|-
|style="background:LightGrey; color:black"|Repetition rate
|style="background:LightGrey; color:black"|Repetition rate
|style="background:WhiteSmoke; color:black"| 200 kHz up to 8000 kHz software controlled
|style="background:WhiteSmoke; color:black"| 200 kHz up to 8000 kHz software controlled
|style="background:WhiteSmoke; color:black"| 200kHz
|style="background:WhiteSmoke; color:black"| 100kHz
|-
|-
|style="background:LightGrey; color:black"|Output power
|style="background:LightGrey; color:black"|Output power

Latest revision as of 09:52, 1 February 2023

Unless anything else is stated, everything on this page, text and pictures are made by DTU Nanolab.

Laser sources

The laser micromachining tool is equipped with two laser sources (1) a picosecond laser (TBW) and (2) a nanosecond laser (IPG). The technical specifications provided by the supplier 3D micromac are shown below. Refer to the Performances to know the measured values of the output power. From 1st of Mar 2017 only the pico second laser is available \ rkch.

Specifications from 3D micromac

Picosecond (TBW) Nanosecond (IPG)
Wavelength 1064nm, 532nm, 355nm 1064nm
Pulse duration 10ps 100ns
Repetition rate 200 kHz up to 8000 kHz software controlled 100kHz
Output power > 50 W @ 1064 nm 100 W
Warm-up time 25min none