'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/ | '''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Thin_film_deposition/Deposition_of_Carbon click here]''' | ||
== Deposition of Carbon == | == Deposition of Carbon == | ||
Carbon can be deposited by DC-sputtering method. So far the process has been tested only using Sputter-System (Lesker): | Carbon can be deposited by DC-sputtering method. So far the process has been tested only using [[Specific Process Knowledge/Thin film deposition/Lesker|Sputter-System (Lesker)]]: | ||
*[[/Deposition of C in Sputter-System Lesker|Deposition of Carbon in Sputter-System (Lesker)]] | *[[/Deposition of C in Sputter-System Lesker|Deposition of Carbon in Sputter-System (Lesker)]] |
Latest revision as of 20:45, 20 December 2022
Feedback to this page: click here
Deposition of Carbon
Carbon can be deposited by DC-sputtering method. So far the process has been tested only using Sputter-System (Lesker):