Specific Process Knowledge/Etch/Etching of Silicon Oxide/SiO2 etch using RIE1 or RIE2/Images of 1SIO2mbr with burned resist mask: Difference between revisions

From LabAdviser
Jump to navigation Jump to search
(New page: ===Etch of SiO2 using the recipe 1SIO2mbr with burned resist as masking material, by Berit Geilman Herstrøm (BGE) from Danchip@DTU=== {| border="2" cellspacing="1" cellpadding="3" align=...)
 
 
(4 intermediate revisions by 2 users not shown)
Line 1: Line 1:
===Etch of SiO2 using the recipe 1SIO2mbr with burned resist as masking material, by Berit Geilman Herstrøm (BGE) from Danchip@DTU===
'''Feedback to this page''': '''[mailto:labadviser@nanolab.dtu.dk?Subject=Feed%20back%20from%20page%20http://labadviser.nanolab.dtu.dk/index.php/Specific_Process_Knowledge/Etch/Etching_of_Silicon_Oxide/SiO2_etch_using_RIE1_or_RIE2/Images_of_1SIO2mbr_with_burned_resist_mask click here]'''
 
=<span style="color:#FF0000"> Both RIE's (RIE1 and RIE2) for silicon based etching has been decommissioned </span> =
* <span style="color:#FF0000"> This information is save because it might be valuable as inspiration for other dry etch systems.
===Etch of SiO2 using the recipe 1SIO2mbr with burned resist as masking material ===
''Berit Geilman Herstrøm (BGE) from Nanolab@DTU''


{| border="2" cellspacing="1" cellpadding="3" align="left"
{| border="2" cellspacing="1" cellpadding="3" align="left"

Latest revision as of 13:07, 6 September 2022

Feedback to this page: click here

Both RIE's (RIE1 and RIE2) for silicon based etching has been decommissioned

  • This information is save because it might be valuable as inspiration for other dry etch systems.

Etch of SiO2 using the recipe 1SIO2mbr with burned resist as masking material

Berit Geilman Herstrøm (BGE) from Nanolab@DTU

Process date: Before 2004
Recipe: 1sio2mbr
Process time: ? min
Mask: Burned resist
Structure size on mask: 3 µm
Etch rate ~120nm/min