Wafer info Mask Material/ Exposed area Tool / Operator Conditioning Recipe Wafer ID Comments
15/12-2014 4" Wafer with travka65 mask AZ standard Si / 65 % Pegasus/jmli 10 minute TDESC clean nanolab/jml/showerhead/SOI/SOI, 96 cyc or 8:00 mins S004745 New showerhead